Free sample articleAdvanced Microstructural Characterization of Plasma-Sprayed Zirconia Coatings Over Extended Length Scales A.A. Kulkarni, A. Goland, H. Herman, A.J. Allen, J. Ilavsky, G.G. Long, and F. De Carlo, Advanced Microstructural Characterization of Plasma-Sprayed Zirconia Coatings Over Extended Length Scales, Journal of Thermal Spray Technology, Vol 14 (No. 2) June 2005, p 239
Sample article from the Journal of Thermal Spray Technology. The complete content of the journal is available by subscription or individual article download at Springerlink.com Springerlink.com. Return to Collections